warm until what temperature?
we say also 1675°c, but quiet, steel is protected by a layer of paper... :redface:say 1650 ° c
I'm not kidding. paper burns in the absence of oxygen, burns, and becomes an excellent insulator)
warm until what temperature?
we say also 1675°c, but quiet, steel is protected by a layer of paper... :redface:say 1650 ° c
I know you have problems with costs and customers a little hard of cervix, but at those temperatures a little thoughts on some alloy steel I would do it... It is good that steels for boilers are generous, but I would not abuse too much of their generosity. . .we say also 1675°c, but quiet, steel is protected by a layer of paper... :redface:
I'm not kidding. paper burns in the absence of oxygen, burns, and becomes an excellent insulator)
I don't know what field you operate, but by forge as the undersigned slag is a punishment!blessed card... .
and blessed scoria, which is saved by many troubles!
of course at those temperatures you have to use the "oven paper":redface:blessed card... .
and blessed scoria, which is saved by many troubles!
or coal paper. . .of course at those temperatures you have to use the "oven paper":redface:
enigma
in practice you are the ones that give us food in short....I in the field that comes before the forge... .
Let's say two steps before the forge.. .
[youtube]3gg9_ztlg4m[/youtube]
[youtube]You're in.[/youtube](I didn't make them... My parents are not available on youtube)
are they not publishable, in the sense that they are top secret, or that they are not publishable for professional decency? :hahahah:(I didn't make them... My parents are not available on youtube)
'stardo.. .are they not publishable, in the sense that they are top secret, or that they are not publishable for professional decency? :hahahah:
mica ora farete south in chi ha la "placca" più lunga??? :hahahahahahahahah: :hahahahahahahah:'stardo.. .
However, they are not available for reasons of secrecy.
You know what department I am...
p355gh en 10028 could do to your case and it is easily weldable.
the supplier tells me that p355gh en 10028 finds it in plates, but not in pipes. Now, one of them is making fun of me, so I'm asking. Are you trying to get me for the cube? because otherwise it must be the other...is a steel for tube bundles from heat exchangers... you should easily find it in pipes